MKP3362X2 Datasheet, PDF (14/17 Pages) Vishay Siliconix – Interference Suppression Film Capacitors MKP Radial Potted Type
MKP 336 2 X2
Vishay BCcomponents
Interference Suppression Film Capacitors
MKP Radial Potted Type
SUB-CLAUSE NUMBER AND
TEST
CONDITIONS
4.9.2 Final measurements
Visual examination
Capacitance
Tangent of loss angle
Insulation resistance
SUB-GROUP C1
COMBINED SAMPLE OF
SPECIMENS OF SUB-GROUPS
C1A AND C1B
4.11 Climatic sequence
4.11.1 Initial measurements
Capacitance
Measured in 4.4.2 and 4.9.2
Tangent of loss angle:
Measured initially in C1A and C1B
4.11.2 Dry heat
Temperature: 110 °C
4.11.3 Damp heat cyclic
Test Db
First cycle
Duration: 16 h
4.11.4 Cold
Temperature: - 55 °C
PERFORMANCE REQUIREMENTS
No visible damage
¦ΔC/C¦ ≤ 5 % of the value measured initially.
Increase of tan δ:
≤ 0.008 for: C ≤ 1 µF or
≤ 0.005 for: C > 1 µF
Compared to values measured initially
As specified in section “Insulation Resistance” of
this specification
4.11.5 Damp heat cyclic
Test Db
remaining cycles
4.11.6 Final measurements
Duration: 2 h
Visual examination
Capacitance
Tangent of loss angle
Voltage proof
1350 Vdc; 1 min between terminations
Insulation resistance
No visible damage
Legible marking
¦ΔC/C¦ ≤ 5 % of the value measured in 4.11.1.
Increase of tan δ:
≤ 0.008 for: C ≤ 1 µF or
≤ 0.005 for: C > 1 µF
Compared to values measured in 4.11.1.
No permanent breakdown or flash-over
≥ 50 % of values specified in section “Insulation
Resistance” of this specification