SPECIFICATIONS
Properties
Electrostatic Decay
Surface Resistivity
Surface Resistivity, Low R.H. Cut-off
High-Voltage Discharge Resistance
Static Shielding
Charged Device Model (CDM) Safety
Current-Carrying Hazard
Corrosivity
Antistat Transfer
Water & Isopropyl Alcohol Extraction
Tests for Antistat Permanence
Sloughing Test
Recyclability
Biodegradability
Volume Conductivity
Shelf Life
Typical Values
Test Procedures/Method
0.01 seconds at 72°F and 11.8% R.H.
107 - 108 ohms/sq. after 11 days at 68°F and 12% R.H.
for surface. 103 - 104 ohms/sq. for buried shielding layer
FED-STD-101, Method 4046
ASTM D257
4% R.H.
Rockwell International Test Report of December 20, 1991
Failure rate 0/5 (no oxide damage in five consecutive tests)
Rockwell International Test Report of December 20, 1991
99.9% attenuation at 10kV; 99.6% attenuation at 30kV
RTG >107 ohms at 86% R.H. or less
103 mA at 110V; 103 mA at 220V
EIA 541, appendix E, capacitive probe test
Rockwell International Test Report of December 20, 1991
ESD from A to Z
Contains 1-3 ppm reducible sulfur
No transfer
Surface resistivity 108 - 109 ohms/square at 74°F
and 36% R.H.
FED-STD-101, Method 3005 for reducible sulfur
Rockwell International Test Report of January 8, 1992
Rockwell International Test Report of January 8, 1992
Negligible surface damage at 10 cycles and <5% of surface
damage at 200 cycles in Taber Abrasion Test.
ASTM D4060 at 70 rpm with CS-17 abrasive-coated
wheels and 1000 grams load
No conductive particles abrased from surface
Complete recyclability of package
Rockwell International Test Report of January 8, 1992
Rockwell International Test Report of January 8, 1992
Biodegradation in or on moist soil
Conductivity from wall to wall as well as across surface
to assure permanence of the antistatic property
Indefinite
Rockwell International Test Report of January 8, 1992
BOARD HANDLER TRAYS
Made in America
© 2005 DESCO INDUSTRIES INC.
Employee Owned
PROTEKTIVE PAK
13520 MONTE VISTA AVENUE, CHINO, CA 91710
PHONE (909) 627-2578, FAX (909) 363-7331
www.protektivepak.com
DRAWING NUMBER
37650
DATE:
7/05